System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Flame Retardant
Material Notes:
This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.
Information provided by CENTROPLAST Engineering Plastics GMBH
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.920
g/cc
ISO 1183
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
62.0
MPa
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield
30.0
MPa
v = 50 mm/min; ISO 527-2
Elongation at Break
10 %
ISO 527-2
Tensile Modulus
1.30
GPa
ISO 527-2
Charpy Impact Unnotched
NB
ISO 179/1eU
Charpy Impact, Notched
1.00
J/cm²
ISO 179/1eA
Electrical Properties
Original Value
Comments
Electrical Resistivity
1.00e+14
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
IEC 60093
Dielectric Constant
2.3
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor
0.0012
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
IEC 60112
Thermal Properties
Original Value
Comments
Thermal Conductivity
0.170
W/m-K
Melting Point
165
°C
10K/min; ISO 3146
Maximum Service Temperature, Air
100
°C
Long Term
130
°C
Short term
Deflection Temperature at 1.8 MPa (264 psi)
55.0
°C
ISO 75-2
Vicat Softening Point
85.0
°C
VST/B/50; ISO 306
Flammability, UL94
V-2
@Thickness 3.00 mm
V-2
@Thickness 6.00 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced
Barlog Plastics KEBAFORM C 901 FA POM Copolymer unreinforced, reduced formaldehyde emission
Barlog Plastics KEBAFORM C 90 M POM Copolymer unreinforced, optimized crystallization
Barlog Plastics KEBAFORM C 130.2 POM Copolymer unreinforced
PCENTR31 / 27982
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.