MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Copper Alloy, UNS C89320, M07 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Casting Yield; Medium – Effect of Section Size, Fluidity, Gassing; Low – Drossing, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing

Typical uses: Washers; Backs for Lined Bearings; Cam Bushings for Diesel Engines; Crankshaft Main Bearings; Deep Well Pump Bowl Bushings; Deep Well Pump Line Shaft Bearings; Electric Motor Bearings; Guide Bushings for Piston Rods; Guide Bushings for Valves; Hydraulic Gland Seals; Main Bearings for Presses; Piston Pin Bearings; Pump Sleeves; Rod Bushings; Rolling Mill Bearings; Seals; Sleeve Bushings (for cranes, etc.); Spacer Bushings (for Pumps, etc.); Wrist Pin Bushings

Applicable Specifications: As Continuous Cast – ASTM B505/B505M; Ingot – ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 70
@Load 500 kg
70
@Load 1100 lb
Tensile Strength >= 241 MPa>= 35000 psifor Standard
 276 MPa40000 psiTypical
Tensile Strength, Yield >= 124 MPa>= 18000 psi0.5% Ext
 138 MPa20000 psi0.5% Ext, Typical
Elongation at Break >= 15 %>= 15 %
 30 %30 %Typical
Tensile Modulus 95.8 GPa13900 ksi
Compressive Strength 138 MPa20000 psi0.1 in. set/in.
Machinability 80 %80 %
Charpy Impact 19.0 J14.0 ft-lbV-Notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000117 ohm-cm0.0000117 ohm-cm14.7% IACS
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 4.67 W/m-K32.4 BTU-in/hr-ft²-°F
Melting Point 927.8 - 1045 °C1702 - 1913 °F
Solidus 927.8 °C1702 °F
Liquidus 1045 °C1913 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.35 %<= 0.35 %
Bismuth, Bi 4.0 - 6.0 %4.0 - 6.0 %
Copper, Cu 87 - 91 %87 - 91 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.090 %<= 0.090 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.30 %<= 0.30 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 5.0 - 7.0 %5.0 - 7.0 %
Zinc, Zn <= 1.0 %<= 1.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC89320x2 / 292573

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.