MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Solef® 60512/0550 and 60512/0150 PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.

Applications: Tape

Features: Copolymer

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 - 1.82 g/cc0.0650 - 0.0658 lb/in³ISO 1183
Water Absorption <= 0.040 %
@Time 86400 sec
<= 0.040 %
@Time 24.0 hour
ASTM D570
Melt Flow 2.0 - 4.5 g/10 min
@Load 10.0 kg,
Temperature 230 °C
2.0 - 4.5 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 - 40.0 MPa
@Thickness 1.50 mm
4350 - 5800 psi
@Thickness 0.0591 in
50 mm/min,Type IV; ASTM D638
Tensile Strength, Yield 30.0 - 40.0 MPa
@Thickness 1.50 mm
4350 - 5800 psi
@Thickness 0.0591 in
50 mm/min,Type IV; ASTM D638
Elongation at Break 50 - 300 %
@Thickness 1.50 mm
50 - 300 %
@Thickness 0.0591 in
50 mm/min,Type IV; ASTM D638
Elongation at Yield 8.0 - 12 %
@Thickness 1.50 mm
8.0 - 12 %
@Thickness 0.0591 in
50 mm/min,Type IV; ASTM D638
Tensile Modulus 1.10 - 1.35 GPa
@Thickness 1.50 mm
160 - 196 ksi
@Thickness 0.0591 in
1.0 mm/min, Type IV; ASTM D638
Coefficient of Friction, Dynamic 0.10 - 0.200.10 - 0.20vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.050 - 0.200.050 - 0.20vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0 - 105.0 - 10CS-10 Wheel, 1000 g, 1000 Cycles; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 41.0 - 50.0 J/g17.6 - 21.5 BTU/lbASTM D3417
Melting Point 170 - 174 °C338 - 345 °F
Crystallization Temperature 144 - 148 °C291 - 298 °FPeak; ASTM D3418
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4484 / 280284

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.