MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Human Articular Cartilage
Categories: Wood and Natural Products

Material Notes: Articular cartilage is located at the bearing surfaces of joints. It has an extremely low coefficient of friction as it serves to provide smooth motion at joints. It also functions as a shock absorber. It is a soft tissue made up of a proteoglycan matrix reinforced with collagen.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 3.40 MPa
Modulus of Elasticity 0.0100 - 0.0210 GPa
Compressive Modulus 0.000700 GPaLateral Condyle of the Femur
Poissons Ratio 0.10Lateral Condyle of the Femur
Coefficient of Friction 0.0020Hip; cartilage vs. cartilage
 
Descriptive Properties
Permeability Coefficient1.18 x 10 -15 M4/N-sLateral Condyle of the Femur

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Human Compact Bone, Haversian System
Silicon Carbide, CVD
Hexcel® HexWeb® HRP - 1/4 - 3.5 Fiberglass/Phenolic Honeycomb
Human Aorta Tissue
Human Skin

PTSXBI12 / 71500

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.