MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aurora Kunststoffe AUROtec® PEEK 90 black PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Product description: AUROtec® PEEK 90 black is a unfilled high end performance compound, semi crystalline for injection molding with easy flow specifications

Typical applications: Thin wall high heat applications, metal substitution

Information provided by Aurora Kunststoffe GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Water Absorption at Saturation 0.45 %Water; ISO 62
Viscosity 90 cP
@Temperature 400 °C
ISO11443
Linear Mold Shrinkage, Flow 0.010 cm/cm
@Temperature 180 °C
60x60x2, MT; ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
@Temperature 80.0 °C
60x60x2, MT; ISO 294-4
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPa50mm/min; ISO 527-1,-2
Elongation at Yield 20 %50mm/min; ISO 527-1,-2
Tensile Modulus 4000 MPa1mm/min; ISO 527-1,-2
Charpy Impact Unnotched NBISO 179-1eU
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 343 °CISO 75,-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75,-1,-2
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 380 °C
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °C
Dry Time 3.00 - 5.00 hour
Moisture Content <= 0.020 %Residual, Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAUROK220 / 249914

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.