MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® TSG-30/4 W PA666-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-30/4 W has the following important properties:
  • High stiffness
  • Excellent flow behavior
  • Excellent oil resistance
  • Very good processing
  • High heat ageing resistance
  • Good surface finish
Application examples are stiff injection molding parts with high resistance against heat ageing such as functional parts in the Automotive Cooling-, Heating-, and Climatic System. Part examples are charged air cooler housings and oil sump housings in the engine compartment.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccDry; ISO 1183
Water Absorption 5.0 %Sim. to ISO 62
Moisture Absorption 2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 110 MPaConditioned; ISO 2039-1
 210 MPaDry; ISO 2039-1
Tensile Strength at Break 125 MPaConditioned; ISO 527-1/-2
 190 MPaDry; ISO 527-1/-2
Elongation at Break 3.0 %Dry; ISO 527-1/-2
 8.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 6000 MPaConditioned; ISO 527-1/-2
 9700 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 21.0 kV/mmConditioned; IEC 60243-1
 25.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 475 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 130 - 150 °CLong Term; ISO 2578
 230 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 155 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Automotive electr. and electronics, lighting
 Cooling and climate control
 Hydraulic systems
Electricals & ElectronicsLighting
FormGranules
Industry & Consumer goodsHeating systems
 Hydraulics & Pneumatics
 Mechanical Engineering
ProcessingInjection Molding
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® GN30 m-Polyphenylene Ether (m-PPE)
Domo TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
BASF Ultramid® A3WG10 BK00564 50% Glass Filled PA66 (Dry)
BASF Ultradur® B 4406 G6 BKQ113 7110 30% Glass Filled PBT
EMS-Grivory Grilon® TSG-30/4 H black 9836 PA666-GF30

PGRH267 / 156976

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.