MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.5 Aramid Honeycomb  (discontinued **)
Categories: Polymer; Thermoset; Aramid; Phenolic

Material Notes: Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)
HexWeb® HRH-36® Flex-Core® aramid paper is reinforced with a high temperature phenolic resin. This product provides good retention of strength for temperatures up to 350°F.

Features: Specifically designed for formability; Retains mechanical properties in the curved condition; Offers cost savings for curved panels.
Applications: The HexWeb® HRH-36® Flex-Core® cell configuration, as opposed to the standard hexagonal cell honeycomb, provides for exceptional formability into compound curvatures with reduced anticlastic curvature and controlled buckling of the cell walls. When formed into tight radii, HexWeb® Flex-Core® provides higher shear strengths than comparable hexagonal cores of equivalent density. HexWeb® Flex-Core® applications exist wherever extreme curvature dictates a flexible cell geometry, e.g. radomes, ducts, leading edges of wings and stabilizers. HexWeb® HRH-36® Flex-Core® offers a weight reduction over higher density NOMEX® cores.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.50 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength 0.444 ksiStabilized, typical value
Shear Modulus 7.10 ksiPlate Shear, W Direction, typical value
 13.8 ksiPlate Shear, L Direction, typical value
Shear Strength 0.128 ksiPlate Shear, W Direction, typical value
 0.236 ksiPlate Shear, L Direction, typical value

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-10/F50 - 5.0 Nonmetallic Flex-Core Honeycomb
Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb
Hexcel® HexWeb® HRP/F50 - 3.5 Nonmetallic Flex-Core Honeycomb
Hexcel® HexWeb® HRP/F50 - 5.5 Nonmetallic Flex-Core Honeycomb
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric

PHEXC353 / 98824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.