This electrically conductive screen ink has been developed for use in printed electronics, notably for membrane switches, flexible circuits, electroluminescent lighting and other applications requiring fine line features. This product features a silver alternate, providing an economical way to achieve resistivity specifications while maintaining market-leading cure times and temperatures. |