MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 3F PAHT® 9875 NT Nylon for Additive Manufacturing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); High Temperature Nylon

Material Notes: High-temperature polyamide unreinforced, natural

Main features: Low influence from moisture and temperature on dimensional stability and electrical properties, compared with PA66

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccISO 1183-3
Water Absorption <= 0.300 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.00300 - 0.00500 cm/cmDIN 16742
Melt Flow 5.10 g/10 min
@Load 2.16 kg,
Temperature 250 °C
pellet
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 80.0 MPa50 mm/min; ISO 527
Elongation at Break 4.00 %50 mm/min, Fmax; ISO 527
Tensile Modulus 3.30 GPa1 mm/min; ISO 527
Charpy Impact Unnotched 135 kJ/m²80x10x4mm; ISO 179 1eU
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 1.00e+12 ohmRonde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 1.00e+12 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
@Time 7.20e+7 sec
Continuous; IEC 60216
 160 °C
@Time 720000 sec
during lifetime
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C80x10x4mm; ISO 75
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 290 °C
Zone 1 260 - 300 °C
Zone 2 260 - 300 °C
Zone 3 260 - 300 °C
Drying Temperature 120 °C
@Time 14400 - 21600 sec
Vacuum
 130 °C
@Time 21600 - 28800 sec
Dehumidifying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUU8722 / 325106

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.