MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Fibracon® PTFE + 55% Bronze + 5% MoS2
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Product characteristics:
  • Excellent wear properties
  • Improved thermal and electrical conductivity
  • Reduced deformation under load
Product applications:
  • High pressure bearings
  • Wear resistant seals

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.70 - 3.90 g/cc0.134 - 0.141 lb/in³ASTM D1457
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62 - 6662 - 66ASTM D1706
Tensile Strength >= 10.0 MPa>= 1450 psiASTM D1457
Elongation at Break >= 50 %>= 50 %ASTM D1457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling Fibracon® PTFE + 15% Glass + 5% MoS2
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
AGC Fluon® RB1211 15% Glass Fiber, 5% MoS2, PTFE Filled Compound
AGC Fluon® PB1211 15% Glass Fiber, 5% MoS2, PTFE Filled Compound
Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2

PROCH9144 / 232847

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.