MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lion SBR 1507 Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: SBR 1507 offers the lowest Mooney viscosity of all SBR 1502 type elastomers. It is a light-colored, general purpose, cold SBR elastomer. It enables a maximum filler loading in rubber applications.

Unique Features:

  • Cold polymerized styrene-butadiene elastomer
  • Lowest Mooney viscosity and light color
Applications:
  • Mechanical rubber goods requiring high filler loading
  • Household products such as floor tiles

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/cc
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Mooney Viscosity 28 - 42
@Temperature 100 °C
28 - 42
@Temperature 212 °F
ML (1+4); ASTM D 1646
Ash <= 0.70 %<= 0.70 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 22.5 - 24.5 %22.5 - 24.5 %Bound; ASTM D5775
 
Descriptive Properties
Content<0.5%Soap, ASTM D5774
 4.9-7.1%Organic acid, ASTM D5774

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLION027 / 317936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.