MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology Silicone Sheet
Categories: Polymer; Thermoset; Silicone

Material Notes: Silicone sheet is FDA approved. Translucent sheet is FDA @ WRC approved. FDA Certificate No. 177.2600

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccSolid Silicone Rubber Sheet
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65Solid Silicone Rubber Sheet
Tensile Strength 5.50 MPa798 psiSolid Silicone Rubber Sheet
Elongation at Break 450 %450 %Solid Silicone Rubber Sheet
Compressive Strength 0.0700 - 0.110 MPa
@Strain 40 %
10.2 - 16.0 psi
@Strain 40 %
Sponge Silicone Rubber Sheet
Compression Set  6.0 %
@Temperature 150 °C,
Time 252000 sec
6.0 %
@Temperature 302 °F,
Time 70.0 hour
Sponge Silicone Rubber Sheet
 25 %
@Temperature 150 °C,
Time 252000 sec
25 %
@Temperature 302 °F,
Time 70.0 hour
Solid Silicone Rubber Sheet
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FSolid Silicone Rubber Sheet
Minimum Service Temperature, Air -40.0 °C-40.0 °FSolid Silicone Rubber Sheet
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock 502 Silicone Sheet Rubber
Overview of materials for Silicone Rubber
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
NUDEC® PET Polyester Sheet
Norplex-Micarta NP101 Phenolic Nylon Laminate Sheet

PPPTEC031 / 133495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.