MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hyosung Topilene HB242P PP
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Topilene ® HB242P is a specially designed polypropylene block copolymer (PP-B, natural colored) that features high modulus(PP-HM) and excellent long-term hydrostatic pressure resistance. It is suitable for underground drainage & sewage pipes and fittings. It is the outcome of HYOSUNG's integrated polymerization and crystallization technology with advanced PP manufacturing process technique.

Typical Applications: Drainage & sewage pipes and fittings (Solid wall & twin wall corrugated pipes system) / Industrial pipes

Features: Excellent long-term hydrostatic pressure resistance / Excellent stiffness and impact strength balance / Enhanced big diameter pipe manufacturing processability / Chemical stability / Environment-friendly

Compliance: The pipes produced with Topilene® HB242P complies with the hydrostatic pressure requirements according to ISO/DIS 15874. It complies with the requirements of FDA 21 CFR 177.1520.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Storage Temperature 40.0 °C104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 31.4 MPa4550 psiASTM D638
Flexural Modulus 1.77 GPa256 ksiASTM D790
Izod Impact, Unnotched NBNBASTM D256
 0.490 J/cm
@Temperature -10.0 °C
0.918 ft-lb/in
@Temperature 14.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 157 °C315 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °FCooling temperature
 200 - 235 °C392 - 455 °Fmixing zone
Feed Temperature 170 - 190 °C338 - 374 °F
Die Temperature 200 - 235 °C392 - 455 °F
Melt Temperature 190 - 225 °C374 - 437 °F
 200 - 235 °C392 - 455 °F
Head Temperature 200 - 235 °C392 - 455 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourair circulated condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hyosung Topilene J800 PP
Hyosung Topilene J340F PP
Hyosung Topilene J340E PP
Hyosung Topilene J301CP PP
Hyosung Topilene HJ746 PP

PHYOS53 / 47939

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.