Description: Nilitop BT FR C3 is an unfilled, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. Key characteristics: - Good overall mechanical performance
- Low moisture absorption
- Colorable
- Good thermal performance
- UL 94 V0 listing at 0.7 mm
Information provided by NILIT. |