MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® 3888 Room Temperature Cure Isotropic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes:
Electrically Conductive Bonders
Loctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditional methods such as solder, are not practical. Electrically Conductive Adhesives are ideal for attaching temperature sensitive components, or providing electrical interconnections on non-solderable substrates, such as plastic and glass.

Loctite offers a complete line of electrically conductive adhesives to meet almost any need including: flexible, heat cure, room temperature cure, screen printable, high adhesion, and rapid cure.

Loctite® 3888 Room Temperature Cure Isotropic Epoxy Adhesive
A room temperature cure adhesive for applications requiring a combination of good mechanical and electrical properties. Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength >= 1000 psiAluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.0010 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear >= 50.0 µm/m-°C
@Temperature 20.0 °C
Glass Transition Temp, Tg 50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 150 °C
 1.00 hour
@Temperature 125 °C
 24.0 hour
@Temperature 23.0 °C
Pot Life 90.0 min
@Temperature 23.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Durabond® E-00CL Epoxy Adhesive
Henkel Loctite® Durabond® M-21HP Epoxy Adhesive
Henkel Loctite® Durabond® E-214HP Epoxy Adhesive
Henkel Loctite® 3335 Epoxy Light Cure Adhesive

PLOCT163 / 51899

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.