MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate

Crastin SK642FR BK851 is a black 15% glass fiber reinforced flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.

Former DuPont product acquired by Celanese in 2022.

Key Words: PBT-GF15FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccISO 1183
Viscosity Number 110 cm³/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527-1/-2
Elongation at Break 3.4 %ISO 527-1/-2
Tensile Modulus 7200 MPaISO 527-1/-2
Flexural Strength 155 MPaISO 178
Poissons Ratio 0.35
Charpy Impact Unnotched 53.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 7.40 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.2
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 32.0 kV/mmIEC 60243-1
Dissipation Factor 0.00196
@Frequency 100 Hz
IEC 62631-2-1
 0.0171
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 218 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 203 °CISO 75-1/-2
Glass Transition Temp, Tg 55.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 0.750 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 5VA
@Thickness 1.50 mm
IEC 60695-11-20
Oxygen Index 32 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °COptimum, Injection
 240 - 260 °CRange, Injection
Mold Temperature 80.0 °COptimum, Injection
 30.0 - 130 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %Injection
Hold Pressure >= 60.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassDNIISO 3795 (FMVSS 302)
Part Marking Code>PBT-GF15FR(17)<ISO 11469
PolymerPBT-GF15 FR(17)
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPBT-GF15FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Crastin® S610SF BK851 Polybutylene Terephthalate (PBT)
Celanese Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
DuPont Mobility and Materials Crastin® T835FRUV NC010 PBT
Edinburg Plastics BGA006 PBT
Edinburg Plastics BGA606 PBT

PDSY5082 / 160909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.