MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F522 Epoxy Resin, T2C145 Carbon Tape  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: T_145-12"-F522; Various Fibers; (145 g/m2)

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  19.7 MPa
@Temperature 24.0 °C
2860 psi
@Temperature 75.2 °F
Dry
 1758 MPa
@Temperature -55.0 °C
255000 psi
@Temperature -67.0 °F
Dry
 1793 MPa
@Temperature 71.0 °C
260100 psi
@Temperature 160 °F
Dry
Tensile Modulus  131.7 GPa
@Temperature 24.0 °C
19100 ksi
@Temperature 75.2 °F
Dry
 132.4 GPa
@Temperature 71.0 °C
19200 ksi
@Temperature 160 °F
Dry
 140 GPa
@Temperature -55.0 °C
20300 ksi
@Temperature -67.0 °F
Dry
Compressive Yield Strength  848 MPa
@Temperature 71.0 °C
123000 psi
@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 1117 MPa
@Temperature 24.0 °C
162000 psi
@Temperature 75.2 °F
Dry
Compressive Modulus  119.3 GPa
@Temperature 71.0 °C
17300 ksi
@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 133.1 GPa
@Temperature 24.0 °C
19300 ksi
@Temperature 75.2 °F
Dry
Shear Strength  38.6 MPa
@Temperature 71.0 °C
5600 psi
@Temperature 160 °F
Short Beam, Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 82.0 MPa
@Temperature 24.0 °C
11900 psi
@Temperature 75.2 °F
Short Beam, Dry
 
Descriptive Properties
Dry Resin Content (%)37-41Prepreg
Flow (%)4-16
Wet Resin Content (%)52Laminate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
Hexcel® HexMC® C / 2000 / R1 Composite SMC
Hexcel® Fibrelam® 2000 Grade 5 Panels for Aircraft Flooring
Hexcel® Fibrelam® 2000 Grade 1 Panels for Aircraft Flooring
Goodfellow Carbon-Carbon Composite

PHEXC140 / 98610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.