Hostacom DYS707N HS1 NAT is an unfilled, impact modified grade that is typically used for automotive pillar applications that require excellent impact/stiffness balance, good flowability, and excellent impact performance at low temperature. Applications : Interior Automotive Applications.Information provided by LyondellBasell. |