MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Honeywell Genetron® HP80 Refrigerant
Categories: Fluid

Material Notes: An interim replacement for retrofitting low- and medium-temperature commercial refrigeration systems. For low- and medium-temperature retrofits.

Chemical Name: Chlorodifluoromethane, Pentafluoroethane, Propane

  • Chemical Notation: CHCIF2CF3CHF2C3 H8

    Information provided by Honeywell

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.12 g/cc
    @Temperature 30.0 °C
    0.0405 lb/in³
    @Temperature 86.0 °F
    Saturated Liquid
    Molecular Weight 101.6 g/mol101.6 g/mol
     
    Chemical PropertiesMetricEnglishComments
    Critical Pressure 42.19 bar31650 torr
    Critical Temperature 75.817 °C168.47 °FASTM D1321
     
    Thermal PropertiesMetricEnglishComments
    Specific Heat Capacity 1.42 J/g-°C
    @Temperature 30.0 °C
    0.340 BTU/lb-°F
    @Temperature 86.0 °F
    Liquid
     0.669 J/g-°C
    @Pressure 0.101 MPa,
    Temperature 30.0 °C
    0.160 BTU/lb-°F
    @Pressure 14.7 psi,
    Temperature 86.0 °F
    Vapor
    Melting Point -103 °C
    @Pressure 0.101 MPa
    -153 °F
    @Pressure 14.7 psi
    Boiling Point -48.9 °C
    @Pressure 0.101 MPa
    -56.1 °F
    @Pressure 14.7 psi

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    PHONWL120 / 179665

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.