MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

INEOS Styrolution Terluran® EHI-7 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: Terluran® EHI-7 is a medium flow, high impact extrusion grade with super high gloss and superior surface aesthetics. Styrolution’s Terluran® EHI-7 is intended for mono or multilayer sheet making it a perfect fit as a substrate for our weatherable Luran® S ASA.
Features: High Impact; High gloss; Outstanding deep draw ability for thermoforming applications; Excellent chemical resistance; Excellent colorability; Enhanced depth of image.
Applications: Sheet extrusion; Thermoforming; Excellent chemical resistance; Coextrusion with Luran® S ASA

Availability: Latin America; North America

Features: Chemical Resistant; Good Colorability; High gloss; High Impact Resistance; Medium Flow; Please Surface Appearance

Uses: Sheet; Thermoforming Applications

Processing Method: Coextrusion; Extrusion; Sheet Extrusion; Thermoforming

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.7 MPa6340 psiASTM D638
Elongation at Break 9.2 %9.2 %ASTM D638
Elongation at Yield 2.9 %2.9 %ASTM D638
Tensile Modulus 2.17 GPa315 ksiASTM D638
Flexural Strength 0.379 MPa
@Strain 5.0 %
55.0 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 2.04 GPa296 ksiASTM D790
Izod Impact, Notched 3.79 J/cm7.10 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FUnannealed; ASTM D648
Vicat Softening Point 100 °C212 °FISO 306/A50
 
Optical PropertiesMetricEnglishComments
Gloss 92 %92 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 218 - 260 °C425 - 500 °F
Drying Temperature 79.4 °C175 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTYS779 / 311472

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.