Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excellent drawability, makes this a very versatile packaging film resin. LL3001.63 is formulated for blown film extrusion. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications: - Freezer Film
- Heavy Duty Bags
- Ice Bags
- Stretch Film
- Trash Bags
Information provided by ExxonMobil |