MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oxygen-free silver-bearing Copper, UNS C10500, H04 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: auto gaskets, radiators, busbars, conductivity wire, contacts, radio parts, winding, switches, terminals, commutator segments, chemical process equipment, printing rolls, clad metals, printed circuit foil.

Test specimens: flat product - 1 mm and 6mm thicknesses.

Similar alloys distinguished only by silver content: 8 oz/ton Ag (UNS C10400), 10 oz/ton Ag (UNS C10500), 25 oz/ton Ag (UNS C10700).

Key Words: AMSIL Copper; Oxygen-free Silver-Copper; ASTM-B-152, QQ-C-502, QQ-C-576
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/ccUNS C10700
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 50
Hardness, Rockwell F 90
Hardness, Rockwell 30T 57
@Thickness 1.00 mm
Flat products
Tensile Strength, Ultimate 345 MPa
Tensile Strength, Yield 310 MPa
Elongation at Break 6.0 %
@Thickness 1.00 mm
in 50 mm
 12 %
@Thickness 6.00 mm
in 50 mm
Modulus of Elasticity 115 GPa
Poissons Ratio 0.307
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %
Shear Modulus 44.0 GPa
Shear Strength 195 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000172 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.385 J/g-°C
Thermal Conductivity 388 W/m-K
@Temperature 20.0 °C
Melting Point <= 1083 °C
Solidus 1083 °C
Liquidus 1083 °C
Annealing Point >= 900 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 475 - 750 °C
Hot-Working Temperature 750 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.95 %Includes Ag
Silver, Ag >= 0.034 %Min 10 troy oz./ton

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zirconium Copper (Amzirc Brand Copper), UNS C15000, TH04 Temper
Copper, UNS C12100
Copper, UNS C12000
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy
Oxygen-free silver-bearing Copper, UNS C10400, H10 Temper flat products

MC10500b6 / 10429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.