Daplen™ EG059AI is a 7% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness. Special Features: - Good scratch resistance
- High flowability
- Low density
- Good surface aesthetics
Applications: Daplen EG059AI has been developed especially for the car industry to be used in automotive interior parts. - Door panels and pockets
- Pillar trims
- Trunk claddings
- Other automotive interior parts
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |