System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Carbon Fiber Reinforced
Material Notes:
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.38
g/cc
Linear Mold Shrinkage, Flow
0.00050
-
0.0015
cm/cm
Linear Mold Shrinkage, Transverse
0.0015
-
0.0030
cm/cm
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
75.0
MPa
@Temperature 120 °C
100
MPa
@Temperature 90.0 °C
115
MPa
@Temperature 60.0 °C
135
MPa
@Temperature 23.0 °C
Elongation at Break
1.3 %
@Temperature 23.0 °C
1.3 %
@Temperature 60.0 °C
1.3 %
@Temperature 90.0 °C
1.4 %
@Temperature 120 °C
Tensile Modulus
14000
MPa
@Temperature 120 °C
15600
MPa
@Temperature 90.0 °C
16800
MPa
@Temperature 60.0 °C
18000
MPa
@Temperature 23.0 °C
Charpy Impact Unnotched
10.0
kJ/m²
Charpy Impact, Notched
5.00
kJ/m²
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
135
°C
Deflection Temperature at 0.46 MPa (66 psi)
145
°C
Deflection Temperature at 1.8 MPa (264 psi)
140
°C
Vicat Softening Point
145
°C
@Load 5.00 kg
Processing Properties
Original Value
Comments
Melt Temperature
280
-
300
°C
Mold Temperature
100
-
120
°C
Drying Temperature
120
-
130
°C
@Time 10800 sec
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, 30% Glass Filled
Overview of materials for Polycarbonate, Molded
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Kotec Carbotex K-30CF10 Polycarbonate, Conductive, 10% Carbon Fiber Reinforced
PLATH9847 / 177543
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.