Hostacom XBR 169G T 3130 is a 15% talc filled impact modified polypropylene, with high impact resistance, good moldability, and good scratch resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 3130 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Interior TrimsInformation provided by LyondellBasell. |