MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Aptek 6106-A/B Epoxy Encapsulant and/or Potting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Optoelectronic grade encapsulant/potting compound – will not attack/cloud polysulphone casings. Lower Tg version, APTEK 6110-A/B, available for ceramic blob-top applications.

Part A is hazy blue. Part B is water clear.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccB Component; ASTM D1475
 1.16 g/ccA Component; ASTM D1475
Viscosity 25 cPB Component; Spindle #1; speed 100 rpm; ASTM D1824
 2000 cPA Component; Spindle #3; speed 10 rpm; ASTM D1824
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85Cured property; ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmCured property; ASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 79.0 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1; Perkin Elmer TMS-2
 175 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2; Perkin Elmer TMS-2
Glass Transition Temp, Tg >= 135 °CCured property; Perkin Elmer TMS-2
Flash Point >= 100 °CB Component; ASTM D92
 >= 200 °CA Component; ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound
BCC Products BC 9060 Silicone RTV Rubber
Abatron 75073 A/B Filled Potting Compound
6106 Aluminum Composition Spec
Aptek 6110-A/B Epoxy Encapsulant and/or Potting Compound

PAPTEK38 / 24200

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.