This grade has typically nice gloss and good surface hardness. Typical applications are sanitary, closures with and without integral hinges.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical / medical applications.
This grade material is UL registered under File E111275.
IMDS 7172624Information provided by SABIC |