MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ohara S-LAH60MQ Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: S-LAH60MQ is an optical glass with smallest dn/dT among current LAH glass types and high refractive indices. Since cars are used in environments where the temperature range can vary widely from below zero in colder climates to more than 50°C inside a car on a summer day, this can cause large refractive index fluctuations within the optical system. While a zoom lens can adjust for these refractive index fluctuations, fixed focused lenses are the most common within the field of Automotive cameras and the necessary adjustments would be nearly impossible. S-LAH60MQ has almost zero dn/dT, unlike many LAH glasses which have large positive dn/dT. This makes S-LAH60MQ an excellent choice not only for automotive applications, but also Projectors, Interchangeable Photographic lenses, and various other applications.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.71 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 51.2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 520
@Load 0.0999 kg
Modulus of Elasticity 95.3 GPa
Modulus of Rigidity 36.6 GPa
Poissons Ratio 0.302
Abrasion 160Aa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.50 µm/m-°C
@Temperature -30.0 - 70.0 °C
 9.80 µm/m-°C
@Temperature 100 - 300 °C
Thermal Conductivity 0.701 W/m-K
@Temperature 35.0 °C
Transformation Temperature, Tg 655 °Cper thermal expansion curve
Softening Point 721 °C107.65 poise; JIS-R3104 and ASTM-C338
Annealing Point 635 °C1013 poise; ASTM-C336
Strain Point 609 °C1014.5 poise; JIS-R3103 and ASTM-C336
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.7881
@Wavelength 2325.42 nm
 1.7943
@Wavelength 1970.09 nm
 1.80135
@Wavelength 1529.58 nm
 1.80854
@Wavelength 1128.64 nm
 1.81125
@Wavelength 1013.98 nm
nt (Hg t line)
 1.81641
@Wavelength 852.11 nm
ns (Cs s line)
 1.82017
@Wavelength 768.19 nm
nA' (K A' line)
 1.82374
@Wavelength 706.52 nm
nr (He r line)
 1.82739
@Wavelength 656.27 nm
nC (H C line)
 1.82843
@Wavelength 643.85 nm
nC' (Cd C' line)
 1.8294
@Wavelength 632.8 nm
nHe-Ne
 1.8338
@Wavelength 589.29 nm
nD
 1.834
@Wavelength 587.56 nm
nd (He D line)
 1.83932
@Wavelength 546.07 nm
ne (Hg e line)
 1.84983
@Wavelength 486.13 nm
nf (H F line)
 1.85116
@Wavelength 479.99 nm
nF' (Cd F' line)
 1.86106
@Wavelength 441.57 nm
nHe-Cd
 1.86281
@Wavelength 435.835 nm
ng (Hg g line)
 1.87401
@Wavelength 404.656 nm
nh (Hg h line)
 1.89407
@Wavelength 365.015 nm
ni (Hg i line)
Abbe Number 36.92ν e
 37.17ν d
Optical Dispersion 0.006608nd-nC; Partial Dispersion
 0.007222nC-nA'; Partial Dispersion
 0.010892ne-nC'; Partial Dispersion
 0.011196nh-ng; Partial Dispersion
 0.011843nF'-ne; Partial Dispersion
 0.011929ne-nC; Partial Dispersion
 0.012981ng-nF; Partial Dispersion
 0.016137nC-nt; Partial Dispersion
 0.017174nC'-nt; Partial Dispersion
 0.022437nF-nC
 0.022735nF'-nC'
 0.02881ng-nd; Partial Dispersion
 0.031262ni-ng; Partial Dispersion
 0.042908ni-nF'; Partial Dispersion
Transmission, Visible 83 %
@Thickness 10.0 mm,
Wavelength 380 nm
Internal Transmission
 89 %
@Thickness 10.0 mm,
Wavelength 390 nm
Internal Transmission
 92.7 %
@Thickness 10.0 mm,
Wavelength 400 nm
Internal Transmission
 95.7 %
@Thickness 10.0 mm,
Wavelength 420 nm
Internal Transmission
 96.8 %
@Thickness 10.0 mm,
Wavelength 440 nm
Internal Transmission
 97.6 %
@Thickness 10.0 mm,
Wavelength 460 nm
Internal Transmission
 98.3 %
@Thickness 10.0 mm,
Wavelength 480 nm
Internal Transmission
 98.9 %
@Thickness 10.0 mm,
Wavelength 500 nm
Internal Transmission
 99.5 %
@Thickness 10.0 mm,
Wavelength 550 nm
Internal Transmission
 99.5 %
@Thickness 10.0 mm,
Wavelength 600 nm
Internal Transmission
 99.5 %
@Thickness 10.0 mm,
Wavelength 650 nm
Internal Transmission
 99.7 %
@Thickness 10.0 mm,
Wavelength 700 nm
Internal Transmission
IR Transmittance 80 %
@Thickness 10.0 mm,
Wavelength 2400 nm
Internal Transmission
 92.7 %
@Thickness 10.0 mm,
Wavelength 2200 nm
Internal Transmission
 96.8 %
@Thickness 10.0 mm,
Wavelength 2000 nm
Internal Transmission
 98.6 %
@Thickness 10.0 mm,
Wavelength 1800 nm
Internal Transmission
 99.5 %
@Thickness 10.0 mm,
Wavelength 1600 nm
Internal Transmission
 99.8 %
@Thickness 10.0 mm,
Wavelength 800 nm
Internal Transmission
 99.8 %
@Thickness 10.0 mm,
Wavelength 900 nm
Internal Transmission
 99.8 %
@Thickness 10.0 mm,
Wavelength 1000 nm
Internal Transmission
 99.8 %
@Thickness 10.0 mm,
Wavelength 1400 nm
Internal Transmission
 99.9 %
@Thickness 10.0 mm,
Wavelength 1200 nm
Internal Transmission
UV Transmittance 8.0 %
@Thickness 10.0 mm,
Wavelength 340 nm
Internal Transmission
 31 %
@Thickness 10.0 mm,
Wavelength 350 nm
Internal Transmission
 56 %
@Thickness 10.0 mm,
Wavelength 360 nm
Internal Transmission
 73 %
@Thickness 10.0 mm,
Wavelength 370 nm
Internal Transmission
 
Descriptive Properties
Acid Resistance, Powder Method, RA(P)3
CCI0.00 B
 1.58 G
 1.58 R
coloring, λ 5340
coloring, λ 80425
Coloring, Internal Transmission λ 0.05336
Coloring, Internal Transmission λ 0.80377
Knoop Hardness Class5
Ohara Code d834372
Ohara Code e839369
Phosphate Resistance, PR1.2
Photoelastic Constant (ß)1.36
Water Resistance, RW(P)1
Weathering Resistance (Surface Method) W(S)max3
Yield Point, At (°C)688per thermal expansion curve

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CZOHARA762 / 281601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.