MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Glastic® SG-200 Polyester Laminate
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Glastic® SG-200 is a Durostone® Glastic laminate and has excellent mechanical properties at high temperatures, but does not meet UL 94 V-0.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 86.0 MPaParallel; ASTM D638
Flexural Strength 131 MPaPerpendicular; ASTM D790
Compressive Strength 248 MPaPerpendicular; ASTM D695
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 20.0 kV/mm
@Temperature 90.0 °C
Perpendicular, air; ASTM D149
 25.0 kV/mm
@Temperature 90.0 °C
Perpendicular, oil; ASTM D149
 50.0 kV/in
@Temperature 90.0 °C
Parallel; ASTM D149
Comparative Tracking Index 500 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CASTM D696
Thermal Conductivity 0.250 W/m-KASTM C177
UL RTI, Electrical 210 °CUL 746 B
UL RTI, Mechanical without Impact 210 °CUL 746 B
 
Descriptive Properties
Colorbrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes SG-200 High Strength/High Temperature Polyester Laminate
AISI 1020 Steel, annealed at 870°C (1600°F)
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic
Evonik Vestodur® GF30-FR5 30% Glass Reinforced, Flame Retardant PBT
Evonik Vestodur® 1003-FR5 Flame Retardant PBT

PROCH9084 / 232787

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.