MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Melt Flow 5.0 - 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
5.0 - 12 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
Hardness, Rockwell R 124124ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Tensile Strength, Yield 55.8 MPa8100 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 3.38 GPa490 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Temperature 22.8 °C
2.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness 1.50 mm
30 - 60 sec
@Thickness 0.0591 in
UL 746
 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
UL 746
 60 - 120 arcs
@Thickness 3.00 mm
60 - 120 arcs
@Thickness 0.118 in
UL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C290 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FASTM D648
Vicat Softening Point 152 °C305 °F120°C/h, 50 N; ASTM D1525
UL RTI, Electrical  80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
 80.0 °C
@Thickness 3.00 mm
176 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
 80.0 °C
@Thickness 3.00 mm
176 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  80.0 °C
@Thickness 1.50 mm
176 °F
@Thickness 0.0591 in
UL 746
 80.0 °C
@Thickness 3.00 mm
176 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0 - 5VA
@Thickness 3.00 mm
V-0 - 5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 293 - 316 °C560 - 600 °F
Middle Barrel Temperature 304 - 327 °C580 - 620 °F
Front Barrel Temperature 316 - 338 °C600 - 640 °F
Melt Temperature 302 - 329 °C575 - 625 °F
Mold Temperature 82.2 - 116 °C180 - 240 °F
Drying Temperature 118 - 124 °C245 - 255 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00127 cm0.000500 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
BLUESTAR PBT 6630 30% Glass Filled
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT

PPOLYQ168 / 160688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.