MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DIAB Divinycell® HT 81 Polymer Foam
Categories: Other Engineering Material; Composite Core Material; Polymer

Material Notes: Divinycell HT is suitable for a very wide range of structural and non-structural applications including aircraft interiors. It is non-hygroscopic, has a reduced environmental impact, superior damage/impact performance and improved dielectric properties.

Continuous operating temperature is -200 to 90°C. The foam can be used in sandwich structures, for outdoor exposure, with external skin temperatures up to 100°C. Normally Divinycell HT can be processed up to 145°C with minor dimensional changes. Maximum processing temperature is dependent on time, pressure and process conditions.

Information Provided by DIAB

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0800 g/ccISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2.80 MPaPerpendicular to the plane; ASTM D1623
Elongation at Break 38 %In Shear; ASTM C273
Tensile Modulus 100 MPaPerpendicular to the plane; ASTM D1623
Compressive Strength 1.50 MPaPerpendicular to the plane; ASTM D1621
Compressive Modulus 105 MPaPerpendicular to the plane; ASTM D1621
Shear Modulus 0.0280 GPaASTM C273
Shear Strength 1.25 MPaASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.2 µin/in-°F
Maximum Service Temperature, Air 90.0 °CContinuous
Minimum Service Temperature, Air -200 °CContinuous
 
Descriptive Properties
Vertical BurnPass60s; FAR 25.853

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB Divinycell® HT 61 Polymer Foam
DIAB Divinycell® HT 101 Polymer Foam
DIAB Divinycell® HCP 30 Polymer Foam
DIAB Divinycell® HCP 50 Polymer Foam
3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa

PDIAA916 / 99154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.