MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ UV Stone Repair Kit Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: ChemSet™ UV Stone Repair Kit - 10 ml Consumer Kit is used when a fast permanent repair is needed to fix scratches, chips, gouges, holes, cracks and nicks on natural and engineered stone. Fast repairs can be completed in less than three minutes. No More Discoloration/Blooming Issues. This easy-to-use UV Kit uses a UV light to cure the adhesive. Without the use of an activator spray as a curing agent you will never have issues with blooming again. Great for lighter colored stones and marbles.

The cure depends on the power of the UV lamp, its spectral output, the distance between the lamp and the components, and the transmission characteristics of the substrates. The cure quoted here was determined using a low power, hand held lamp. Most industrial UV lamps would give faster cure rate.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 lb/galuncured
Viscosity 1000 - 1500 cP
@Temperature 25.0 °C
uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60
Tensile Strength 1450 - 1500 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Dielectric Strength 12000 V/mil
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.484cured
Transmission, Visible 98 %cured
 
Descriptive Properties
Colorcolorless, uncured
Cure Wavelength365-420 nm
Fixture Time3.5 sec, low power 3.5 mW/cm2 lamp
Tack Free Time3.5 sec. 33mW/cm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI976 / 232159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.