MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EB412 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: WESTLAKE polyethylene EB412 is a low-density polyethylene with very good optical and strength properties, and has an enhanced stabilization package for increased thermal stability during extrusion. This material is an excellent choice for bakery films and food packaging applications.

    Application/Uses
  • General purpose clarity packaging
  • Medium duty produce bags
  • Bakery bags
  • Bags for textile items

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Very good optical and strength properties, and an enhanced stabilization package for increased thermal stability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D1505
Thickness 1.25 mil
Melt Flow 2.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 350 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Dart Drop 100 g/milASTM D1709
Film Tensile Strength at Break, MD 3500 psiASTM D882
Film Tensile Strength at Break, TD 2700 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 4.2 %ASTM D1003
Gloss 76 %at 45º; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 390 °Fwith BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake EF923 Low Density Polyethylene
Westlake HM 5004 High Density Polyethylene
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
Westlake EC477AA Low Density Polyethylene

PWESF032 / 84469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.