MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stability

Process Stability. 3662 features excellent processability and the good physical properties necessary for fibers and multifilaments.

FDA. 3662 complies with all applicable FDA regulations for food contact applications.

Recommended Applications. TOTAL Polypropylene 3662 is recommended for staple fibers and bulk continuous filament (BCF) yarns.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Melt Flow 10.2 g/10 minASTM D1238, L
 
Mechanical PropertiesOriginal ValueComments
Elongation at Yield 70 %ASTM D3218
Tensile Modulus 1790 MPaASTM D638
Tenacity 3.50 g/denierASTM D3218
Flexural Modulus 1655 MPaASTM D790
Flexural Stiffness 1310 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade
Total 3761 Polypropylene, Extrusion Grade
Total PPS 15080 S01 Polypropylene, Homopolymer Fiber Grade
Amco PRIMATOP PP HOMO 038X Fiber Grade Polypropylene
NatureWorks® Ingeo™ 5051X Fiber Grade PLA

PTOTAL814 / 130539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.