MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Stretch-Vac® 2000 Vacuum bagging film
Categories: Polymer; Film

Material Notes: Description: Sealant tape. Ideally suited to aerospace applications.

Features & Benefits:

  • Soft, co-extruded, ultra high elongation, multi layered film, produced from a modified polyamide resin
  • Easily conformable for complex contoured parts, formulated to be less affected by environmental changes and remains flexible in low humidity conditions
  • Recommended as a bagging film for advanced composite fabrication, when a dependable, conformable, soft, stretchable bag is required
  • Fewer pleats are needed when vacuum bagging either complex or simple contoured parts, due to its unique characteristics
  • Manufactured using advanced “state-of-the-art” blown film technology
  • Can be heat seamed to meet any custom shape requirements.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 microns
 75.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 15000 psiASTM D882
Elongation at Break 400 %ASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
 
Descriptive Properties
ColorRed and transparent
Yield11.6 m2/kg75 µm
 17.3 m2/kg50 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTED299 / 180601

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.