MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AK Steel 309S Austenitic Stainless steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic when cold worked. AK Steel 309S is identical to AK Steel 309, except for a lower carbon content that minimizes carbide precipitation and improves weldability.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.01 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85Annealed
Tensile Strength, Ultimate 621 MPaAnnealed
 145 MPa
@Temperature 871 °C
 441 MPa
@Temperature 538 °C
 545 MPa
@Temperature 204 °C
Tensile Strength, Yield 310 MPa
@Strain 0.2 %
Annealed
 120 MPa
@Strain 0.2 %,
Temperature 871 °C
 200 MPa
@Strain 0.2 %,
Temperature 538 °C
 262 MPa
@Strain 0.2 %,
Temperature 204 °C
Elongation at Break 45 %in 2 inches, Annealed
 38 %
@Temperature 538 °C
in 2 inches
 46 %
@Temperature 204 °C
in 2 inches
 50 %
@Temperature 871 °C
in 2 inches
Modulus of Elasticity 200 GPa
Izod Impact 140 JV-Notch (Annealed)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000780 ohm-cm
Magnetic Permeability <= 1.02H = 200 Oersted, Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.9 µm/m-°C
@Temperature 0.000 - 100 °C
 18.0 µm/m-°C
@Temperature <=649 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 15.6 W/m-K
@Temperature 100 °C
 18.7 W/m-K
@Temperature 500 °C
Melting Point 1399 - 1454 °C
Solidus 1399 °C
Liquidus 1454 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 22 - 24 %
Iron, Fe 58.095 - 66 %As Remainder
Manganese, Mn <= 2.0 %
Nickel, Ni 12 - 15 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 309S Stainless Steel
AISI Type 309S Stainless Steel, annealed, sheet
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition A
309 Stainless Steel, annealed, sheet
AK Steel 304 Austenitic Stainless steel

NAKS111 / 14714

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.