MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewable raw materials. Grivory XE 4027 natural is free of halo-gens and red phosphorus. RoHS: Grivory XE 4027 natural is in compliance with RoHS (2002/95/EC, Restriction of Hazardous Substances). WEEE: Parts produced from Grivory XE 4027 natural are not subject to "selective treatment" according the Directive 2002/96/EC on Waste Electrical and Electronic Equipment. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide. The main distinguishing features of Grivory HT, when compared to other poly-amides, are its good performance at high temperatures providing parts which are stiffer, stronger, have better heat distortion and dimensional stability as well as excellent chemical resistance and low moisture absorption. Grivory XE 4027 natural is especially suitable for injection molded components in electrical and electronic applications which require a flame class acc. UL 94 V-0. The material is suitable for lead-free SMT reflow soldering acc. e.g. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL1 are achievable.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Water Absorption 2.3 %ISO 62
Moisture Absorption 0.900 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 235 MPadry; ISO 2039-1
 235 MPaconditioned; ISO 2039-1
Tensile Strength at Break 130 MPadry; ISO 527-1/-2
 130 MPaconditioned; ISO 527-1/-2
Elongation at Break 2.0 %dry; ISO 527-1/-2
 2.0 %conditioned; ISO 527-1/-2
Tensile Modulus 10000 MPaconditioned; ISO 527-1/-2
 10000 MPadry; ISO 527-1/-2
Charpy Impact Unnotched 50.0 kJ/m²dry; ISO 179/1eU
 50.0 kJ/m²conditioned; ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²dry; ISO 179/1eA
 8.00 kJ/m²conditioned; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmdry; IEC 60093
 1.00e+11 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 33.0 kV/mmdry; IEC 60243-1
 33.0 kV/mmconditioned; IEC 60243-1
Comparative Tracking Index 600 Vconditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-1/-2
Melting Point 295 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °Clong term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 260 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 155 °CISO 75-1/-2
Flammability, UL94 V-0IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Exterior
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
 Mobile phones and other portable devices
FormGranules
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Hydrolysis resistant
Special CharacteristicsFlame retardant
 Improved heat resistance
 Improved UV resistance (outdoor use)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30
EMS-Grivory Grivory® HT XE 3996 PA*-GF30
Arkema Rilsan® HT CZM 30 BLACK TLD PA-GF30
EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 43)
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30

PGRH367 / 157076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.