MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mitsubishi Iupital® A10-03 Copolymer Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: High anticreep. Standard 2. Iupital is a copolymer-type acetal resin produced with our proprietary manufacturing process. Used in a wide range of industries, Iupital is ideal for precision machinery, automobile, OA and electronics applications. Well-balanced mechanical properties and high fatigue resistance. Excellent anticreep properties. Excellent low friction and anti-wear properties. Wide range of operating temperatures. High oil and organic chemical resistance. Excellent thermal stability in molding.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 0.220 %
@Temperature 23.0 °C
0.220 %
@Temperature 73.4 °F
60% RH
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 3.00 mm
0.022 in/in
@Thickness 0.118 in
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 67.0 MPa9720 psiISO-527-1,2
Elongation at Break 35 %35 %ISO 527-1,2
Elongation at Yield 9.0 %9.0 %ISO 527-1,2
Tensile Modulus 2.90 GPa421 ksiISO 527-1,2
Flexural Strength 94.0 MPa13600 psiISO 178
Flexural Modulus 2.75 GPa399 ksiISO 178
Charpy Impact Unnotched 28.0 J/cm²133 ft-lb/in²ISO 179-1,2
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179-1,2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 168 °C334 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FISO 75-1,2
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General
Mitsubishi Iupilon® TMB 1615 PC/ABS
Mitsubishi Hostaphan® RN, 190 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Mitsubishi Hostaphan® RN, 23 micron Nominal Thickness Universal Polyethylene Terephthalate Film

PMITSU9152 / 191825

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.