Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivory GVX-5H natural has an optimized flowability and is suitable for injection molding technical parts, exhibiting exceptional characteristics even after moisture absorption:- high stiffness and strength
- high dimensional stability, very low warpage
- good chemical resistance
- very good surface finish
Grivory GVX-5H natural is the economical alternative to die-cast alloys.Information provided by EMS Grivory |