MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
AK Steel 316L Austenitic Stainless steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.

Information provided by AK Steel

Key Words: UNS S31603
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.99 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 79
Tensile Strength, Ultimate 558 MPa
Tensile Strength, Yield 290 MPa
@Strain 0.2 %
Elongation at Break 50 %in 2 inches
Tensile Modulus 193 GPa
Poissons Ratio 0.25Calculated
Shear Modulus 77.0 GPatorsion
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cm
Magnetic Permeability <= 1.02H = 200 Oersted, Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 100 °C
 19.9 µm/m-°C
@Temperature <=871 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 100 °C
 21.4 W/m-K
@Temperature 500 °C
Melting Point 1371 - 1399 °C
Solidus 1371 °C
Liquidus 1399 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 16 - 18 %
Iron, Fe 62.045 - 72 %As Remainder
Manganese, Mn <= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
Nickel, Ni 10 - 14 %
Nitrogen, N <= 0.010 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 316L Stainless Steel, annealed sheet
AISI Type 316L Stainless Steel, annealed bar
AISI Type 316L Stainless Steel, annealed plate
AK Steel 316 Austenitic Stainless steel
AISI Type 316L Stainless Steel, annealed and cold drawn bar

NAKS113 / 14716

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.