MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8235G HS BK 102 50% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under load is excellent. It is available in natural, black, weather resistance and pigmented versions.

Applications: Ultramid 8235G HS BK-102 is generally recommended for applications such as power tool housings, cattle ear taggers, luggage frames, fans and pressure regulator housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Moisture Absorption at Equilibrium 1.4 %50% RH; ISO 62
 4.8 %Saturation; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaISO 527
Elongation at Break 6.0 %ISO 527
Tensile Modulus 8910 MPaISO 527
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 305 °C
Mold Temperature 80.0 - 95.0 °C
Drying Temperature 80.0 °C
Dry Time 2 - 4 hour
Moisture Content >= 0.060 %
Injection Pressure 35.0 - 125 MPa
 
Descriptive Properties
ColorBK 102
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8235G HS BK 102 50% Glass Filled PA6 (Dry)
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)
Envalior Akulon® K224-G0 PA6-GF50, Conditioned, 50% Glass Filled
EMS-Grivory Grilon® BG-50 PA6-GF50
Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled

PBASG0473 / 132106

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.