MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® A 2457 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol A 2457 is an anionic polyacrylic dispersion. It is suitable as a binder in the formulation of water-reducible two-component coatings and sealers for mineral substrates and reactive resins (EP, PU).

Properties / Applications: Because of its outstanding mechanical and chemical resistance properties the product is ideally suited for the formulation of sealers for mineral substrates and reactive resins (EP, PU). Combination with other water-reducible binders is possible. Because of the many potential combination products, compatibility must always be tested. As with any product, use of Bayhydrol A 2457 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Volatiles 58.5 - 61.5 %1g/1h/125 °C/convection oven
pH 7.5 - 9.01:3 in demineralized water
Viscosity <= 100 cPD= approx. 42 s-1
 
Descriptive Properties
Content2.5%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayhydrol® A 145 Polyurethane Coating
Covestro Bayhydur® XP 2451/1 Polyurethane Coating

PCOVEST0152 / 201935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.