MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Matexcel CER-0024 Mg/Sr/Zn Doping calcium silicate
Categories: Other Engineering Material

Material Notes: Adding Mg2+, Sr2+ and Zn2+ ions to Ca-Si-based/Ca-P-based bioceramic scaffolds can not only improve the chemical stability of the original ceramic scaffold materials, but also enhance their biological activity and biocompatibility.

calcium silicate; Doping calcium silicate

Application: This product can be used as a preparation of Ca-Si-based bioceramics, coatings and composite materials. After sterilization, it can also be used for plastic surgery and cosmetic surgery, dental surgery, repair due to trauma, tumor, inflammation, bone disease, etc. Bone defects and bone fusion.

Morphology: Needle-like, short rod powder

Key Words: Synonyms: calcium silicate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 5.0 - 20 µm
Storage Temperature 20.0 °C
 
Descriptive Properties
ComponentsCaxMgySrzSiO
Purity>99% Heavy metal: <4ppm As: <1ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1360 / 299991

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.