MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optimized for low phosphate release, to limit the formation of deposits on electrical contacts. The material has a red-brownish natural color.

Key characteristics:

  • UL 94 V0 at 1.5 mm
  • High strength and stiffness
  • RTI listing up to 110°C at 0.4 mm
  • High CTI: 600V
  • Low phosphate release

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ASTM D792, ISO 1183
Water Absorption 0.80 %0.80 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 5.5 %5.5 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inEuronil
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inEuronil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 150 MPa21800 psiISO 527, ASTM D638
Elongation at Break 2.5 %2.5 %
Tensile Modulus 9.00 GPa1310 ksiISO 527, ASTM D638
Flexural Yield Strength 210 MPa30500 psiISO 178, ASTM D790
 125 MPa
@Temperature 90.0 °C
18100 psi
@Temperature 194 °F
ISO 178, ASTM D790
Flexural Modulus 8.20 GPa1190 ksiISO 178, ASTM D790
 4.30 GPa
@Temperature 90.0 °C
624 ksi
@Temperature 194 °F
ISO 178, ASTM D790
Izod Impact, Notched (ISO)  7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 8.50 kJ/m²
@Temperature 23.0 °C
4.04 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 3.80 J/cm²18.1 ft-lb/in²ISO 179
 2.70 J/cm²
@Temperature -30.0 °C
12.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 20.0 kV/mm
@Thickness 2.00 mm
508 kV/in
@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index  500 V
@Thickness 3.20 mm
500 V
@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
 500 V
@Thickness 3.20 mm
500 V
@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75, ASTM D648
Vicat Softening Point 250 °C482 °F49 N; ISO 306, ASTM D1525
 255 °C491 °F9.8 N; ISO 306, ASTM D1525
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Oxygen Index 29 %29 %ASTM D2863
Glow Wire Flammability Index  960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 694-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 694-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 285 °C527 - 545 °F
Zone 1 260 - 280 °C500 - 536 °Fhopper
Zone 2 260 - 280 °C500 - 536 °F
Zone 3 270 - 280 °C518 - 536 °F
Zone 4 275 - 285 °C527 - 545 °F
Melt Temperature 275 - 290 °C527 - 554 °FDo not melt above 290°C
Mold Temperature 90.0 - 110 °C194 - 230 °FPreferred
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 4 hour4 hour
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi
 
Descriptive Properties
Clamping Forcein tons, 0.7 times the projected surface area in cm2
Flammability RatingSEFMVSS No. 302, 355x100x1 mm
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Holding Pressure90 MPa
Needle TestOKIEC 695-2-2, 1 or 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens)
Celanese Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)

PLBN39 / 50428

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.