System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 20% Glass Fiber Filled
Material Notes:
15% Glass Fiber Reinforced, Good surface
Information provided by E-Polymers Co. Ltd.
Key Words:
Polyamide 66
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.23
g/cc
ASTM D792
Water Absorption
0.90 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage
0.0050
cm/cm
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
120
ASTM D786
Tensile Strength, Yield
130
MPa
ASTM D638
Elongation at Break
4.0 %
ASTM D638
Flexural Yield Strength
200
MPa
ASTM D790
Flexural Modulus
5.60
GPa
ASTM D790
Izod Impact, Notched
0.700
J/cm
ASTM D256
Izod Impact, Unnotched
60.0
J/cm
@Thickness 3.20 mm
ASTM D256
Thermal Properties
Original Value
Comments
CTE, linear
40.0
µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point
260
°C
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi)
240
°C
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
ASTM D648
Flammability, UL94
HB
Processing Properties
Original Value
Comments
Processing Temperature
280
-
300
°C
Mold Temperature
80.0
-
100
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre
Plastcom SLOVAMID 66 GF 10 PA66, 10% glass fibre
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)
Plastcom SLOVAMID 66 GF 15 Polyamide 66, 15% Glass Fiber
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Conditioned)
PEPOLY06 / 36308
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.