MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Kennametal Stellite Denertia™ N19 Nickel Dental Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Denertia™ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.

This alloy is Beryllium and Cadmium free

Information provided by Kennametal Stellite™

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 200200
Tensile Strength, Ultimate 640 - 700 MPa92800 - 102000 psi
Tensile Strength, Yield 360 - 480 MPa52200 - 69600 psiProof Stress
Elongation at Break >= 13 %>= 13 %
Flexural Modulus 170 GPa24700 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.1 µm/m-°C
@Temperature 20.0 - 600 °C
7.83 µin/in-°F
@Temperature 68.0 - 1110 °F
Melting Point 1300 - 1370 °C2370 - 2500 °F
Solidus 1260 - 1270 °C2300 - 2320 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 24 %24 %
Cobalt, Co <= 1.0 %<= 1.0 %
Iron, Fe 1.0 %1.0 %
Molybdenum, Mo 9.5 %9.5 %
Nickel, Ni >= 60.95 %>= 60.95 %as balance
Niobium, Nb (Columbium, Cb) <= 1.0 %<= 1.0 %
Other <= 0.50 %<= 0.50 %
Silicon, Si <= 2.0 %<= 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Denertia™ C14 Cobalt Chromium Dental Alloy
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy
AgPd-4 Precious dental alloy
HGC-1 Precious dental alloy
Kennametal Stellite Denertia™ C13 Cobalt Chromium Dental Alloy

NSTA4967 / 159899

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.