MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Europrene® SOL T 9326 Styrene - Isoprene Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Europrene® SOL T 9326 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 30% weight and diblock content is 15%. A non-staining, TNPP free antioxidant system is added during the production process.

Key Features: Europrene® SOL T 9326 is an easy processable grade, characterized by low viscosity, high cohesion and improved thermal stability .

Main Applications: The polymer is designed for highly demanding hot melt adhesive applications.

Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
Brookfield Viscosity 300 cPToluene sol., 25% wt; ASTM D1084
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D2240
Tensile Strength at Break 22.0 MPaASTM D412
Elongation at Break 1000 %ASTM D412
300% Modulus 0.00180 GPa
@Strain 300 %
ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer
Versalis Europrene® SOL T 9131 Styrene - Isoprene Block Copolymer
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Versalis Europrene® SOL T 9113 Styrene - Isoprene Block Copolymer
Versalis Europrene® SOL T 9133 Styrene - Isoprene Block Copolymer

PENG217 / 124611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.