MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Adamas Adalon® 301 PTFE, 10% Graphite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.14 - 2.16 g/ccASTM D792
Deformation 5.0 - 7.5 %Permanent deformation after 24 hrs @ 23°C; ASTM D621
 9.0 - 10.5 %ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56 - 62ASTM D2240
Tensile Strength at Break >= 19.0 MPaASTM D4894
Elongation at Break >= 210 %ASTM D4894
Coefficient of Friction, Dynamic 0.080 - 0.10ASTM D1894
Coefficient of Friction, Static 0.060 - 0.080ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmASTM D257
Surface Resistance 1.00e+9 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.390 W/m-KASTM C 177
Melting Point 327 °CDSC
Maximum Service Temperature, Air 260 °CDSC
Minimum Service Temperature, Air -180 °CDSC
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Adamas Adalon® 252 PTFE, 28% Glass Fiber
Adamas Adalon® 237 PTFE, 25% Glass Fiber
Adamas Adalon® 415 PTFE, 10% Organic Filler
Adamas Adalon® 413 PTFE, 20% PPS
Adamas Adalon® 410 PTFE+ PEEK

PHADAM026 / 147212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.