MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) TEDUR® L 9107-7 PPS, 40% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Base Polymer: Polyphenylene Sulfide

Filler/Additive System: 40% glass fibers

Special Features: Injection molding grade, high toughness, reduced flash, increased burst strength, low odor

Market Segment: Automotive, Machinery, various

Application Area: Pump components

Typical Applications: housings, pump impellers, high pressure vessels

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaISO 527
Elongation at Break 1.8 %ISO 527
Tensile Modulus 15500 MPaISO 527
Flexural Strength 285 MPaISO 178
Flexural Modulus 14500 MPaISO 178
Flexural Strain at Break 2.2 %Flexural deflection at max force; ISO 178
Izod Impact, Unnotched (ISO) 45.0 kJ/m²ISO 180/1U
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+12 ohmDIN EN 62631-3-2
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 275 °CISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.50 mm
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
passed; DIN EN 60695
 960 °C
@Thickness 2.00 mm
passed; DIN EN 60695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 320 - 340 °CInjection molding
Mold Temperature >= 140 °CInjection molding
Drying Temperature 130 - 140 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyphenylene Sulfide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Mocom (ALBIS) TEDUR® L 9510-1 PPS, 40% Glass Fiber Reinforced
Mocom (ALBIS) TEDUR® L 9107-1 PPS, 40% Glass Fiber Reinforced
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)
Chevron Phillips Xtel® XE4050BL Polyphenylene Sulfide Alloy

PALBIS8345 / 242404

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.