MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Pocan® C 3230 XF 000000 PBT+PC, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT+PC 30% glass fiber, improved flowability reduced warpage, good surface quality

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Filler Content 30 %Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 cm/cmPlaque 60 x 60 x 2mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmPlaque 60 x 60 x 2mm; ISO 294-4
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 2.6 %5 mm/min; ISO 527-1,-2
Tensile Modulus 7500 MPa1 mm/min; ISO 527-1,-2
Flexural Strain at Yield 2.7 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 45.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 225 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 120 °CMethod Af; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 165 °CMethod Bf; ISO 75-1,-2
Shrinkage, MD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
Shrinkage, TD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CPlaque 60 x 60 x 2mm
Mold Temperature 80.0 °CPlaque 60 x 60 x 2mm
Hold Pressure 60.0 MPaPlaque 60 x 60 x 2mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® A 3131 000000 PBT+PC, 30% Glass Fiber Reinforced
Avient Edgetek® PC-30GF/000 Polycarbonate (PC), Glass Filled
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy
Envalior Arnite® TV4 640 (PBT+PC) - GF20

PLANW9036 / 208433

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.